SKAPS TN 160 – GEOCOMPOSITE – ENGLISH UNITS

Description

SKAPS TN 160 – GEOCOMPOSITE – ENGLISH UNITS: SKAPS TRANSNETTM Geocomposite consists of SKAPS Geonet made from HDPE resin with nonwoven polypropylene geotextile fabric heat-bonded on one side or both sides of Geonet.
PROPERTY TEST METHOD UNIT VALUE VALUE QUALIFIER
GEONET
Thickness ASTM D 5199 mil 150 150 MAV(3)
Carbon Black ASTM D 4218 % 2.00 2.00 MAV
Tensile Strength ASTM D 7179 lb/in 30 30 MAV
Melt Flow ASTM D 1238(2) g/10 min 1.00 1.00 Maximum
Density ASTM D 1505 g/cm3 0.94 0.94 MAV
Transmissivity(1) ASTM D 4716 gal/min/ft (m2/sec) 4.83 (1.0 x 10-3) 4.83 (1.0 x 10-3) MAV
GEOCOMPOSITE 6 oz/yd2 8 oz/yd2
Ply Adhesion ASTM D 7005 lb/in 1.00 1.00 MAV
Transmissivity(1) DS ASTM D 4716 gal/min/ft (m2/sec) TN 160-2-6 TN 160-2-8
0.48 (1.0 x 10-4) 0.48 (1.0 x 10-4) MAV
Transmissivity(1) SS ASTM D 4716 gal/min/ft (m2/sec) TN 160-1-6 TN 160-1-8
2.42 (5.0 X 10-4) 2.42 (5.0 X 10-4) MAV
GEOTEXTILE
Fabric Weight ASTM D 5261 oz/yd2 6 8 MARV(4)
Grab Tensile ASTM D 4632 lb 160 225 MARV
Grab Elongation ASTM D 4632 % 50 50 MARV
Trapezoid Tear ASTM D 4533 lb 65 90 MARV
CBR Puncture ASTM D 6241 lb 450 600 MARV
Water Flow(5) ASTM D 4491 gpm/ft2 125 100 MARV
Permittivity(5) ASTM D 4491 sec-1 1.63 1.26 MARV
Permeability(5) ASTM D 4491 cm/sec 0.30 0.30 MARV
AOS ASTM D 4751 US Sieve 70 80 MaxARV
  Notes: (1) Transmissivity was measured using water at 21 ± 2 ° C (70 ± 4) ° C with a gradient of 0.1 and a confining pressure of 1,000 psf between steel plates after 15 minutes. Values may vary with individual labs. DS – Double-Sided, SS -Single-Sided (2) Condition 190/2.16 (3) Minimum average value. (4) MARV is statistically defined as the mean minus two standard deviations, and it is the value that is exceeded by 97.5% of all the test data. (5) At the time of manufacturing. Handling may change these properties.